Buyer Research · Floor and tread compatibility

Metal chips in caster treads: why a wheel material label does not predict floor damage

A caster that is nominally “floor-protective” can become a floor-damaging contact if hard chips or weld debris become trapped in its tread. The decision is not simply PU versus rubber: published guidance, a field case and specific wheel constructions point to different outcomes.

Decision first

Do not approve a caster for metal-chip routes from the material name alone. Qualify the exact tread compound, hardness and profile against the actual chip type and floor finish, and control the debris on the route. A softer tread helped in one reported welding-shop case, but another manufacturer's floor-selection table recommends rubber for chip-covered floors, while a specific crowned TPR construction is advertised as rejecting metal shavings. These are not interchangeable material-class claims.

The practical failure chain is: hard debris is collected or embedded in the tread → the debris becomes part of the wheel-floor contact → repeated rolling/turning can score or groove the floor → the resulting track can affect AGV guidance and safety. This is a documented case mechanism, not a universal prediction for every chip or wheel.

What independent sources actually say

Source and locationOriginal evidenceWhat it does not prove
ELESA+GANTER — Castors and Wheels: Technical Data, Copyright 2018, printed p.17 §5.1 and floor/covering tableIts table maps “With chips/obstacles” to rubber covering. The surrounding text says floor nature, obstacles and machining residues affect wheel choice and calls for particular care.No chip material, particle size, concentration, rubber compound, hardness or comparative field test is specified. “Rubber” is a screening recommendation, not a guarantee against embedding.
Caster Connection — “Bodyweld: The Right Wheel for the Application”, Challenge / Solution / ResultsA body-weld shop reported weld dust, slag and metal shavings collecting in rubber treads and becoming embedded until the wheel-floor contact was effectively metal. The wheels cut a permanent floor groove. The supplier diagnosed the replacement polyurethane tread as too hard to deflect debris and recommended a softer PU tread; the case reports no further debris pickup after replacement.The same case says the AGVs were typically loaded about 450 kg over their caster rating. It is a supplier-reported single-site case, not a controlled comparison isolating tread hardness, nor proof that all soft PU grades reject all chips.
Caster Technology Corporation — “Wheels”, TMP Series, “Soft Rubber on Polyolefin, Crowned Tread”The named construction is a soft thermoplastic-rubber tread permanently bonded to a ribbed polyolefin core; the manufacturer says this specific series rejects floor debris such as metal shavings.The page does not disclose chip size, debris concentration, test route, load, wear duration or independent validation. The claim belongs to TMP, not to every rubber or TPR wheel.
Sika — General Maintenance for New Floor Systems: Sikafloor Maintenance Guidelines, p.1Sika says dirt and debris combined with constant wheel traffic can act like sandpaper, dulling, scratching or gouging floor coatings; it recommends condition-based sweeping, repair of scratches/gouges and avoiding dragging heavy equipment.This is floor-system maintenance guidance, not a caster-material ranking or a test of metal-chip embedding.
ErgonArmor — Technical Bulletin T21-010, 2021-08-31, p.1, “Maintenance Suggestions”For its epoxy and urethane floor coatings, it says abrasive dirt such as sand or metal chips should be dry-swept at least daily; it also advises minimizing scraping/sliding heavy machinery and sharp objects.The frequency is specific to the cited coating maintenance bulletin and site conditions; it is not a universal legal or engineering cleaning interval.

Why the apparent material conflict is not a contradiction to average away

ELESA+GANTER's broad table recommends rubber for a floor with chips or obstacles. Caster Connection's welding-shop narrative, however, describes a rubber tread collecting weld debris and a hard PU tread allowing slag and chips to embed; it reports a better outcome after moving to a softer PU tread. Caster Technology separately attributes debris rejection to one specific soft TPR-on-polyolefin crowned design. These sources do not test the same compounds, chip geometry, loads or floor conditions. They therefore cannot support a universal ranking such as rubber > PU, PU > rubber, or softer is always better.

The important distinction is between a material family and a finished tread construction. Compound formulation, hardness, elastic recovery, tread profile and the actual particle's shape/sharpness can change whether debris is displaced, trapped, embedded or retained. The public sources do not provide a common test method or enough data to quantify those effects. The field case also contains an overload confounder: because the AGVs exceeded the caster rating, its outcome cannot be attributed to hardness alone.

Floor damage is a second system, not just a wheel property. Sika's description of debris plus wheel traffic as a sandpaper mechanism and ErgonArmor's daily dry-sweep recommendation show why even a well-matched tread should not be treated as permission to leave metal chips on the route. A caster substitution cannot replace housekeeping or floor repair.

Buyer decision path

  1. Describe the contaminant. Identify whether the route contains fine grinding dust, short sharp swarf, long curled chips, weld slag/spatter, abrasive grit or mixed debris. Record typical and worst-case size, sharpness, amount and whether chips are loose, oily or hot. Do not treat these as equivalent.
  2. Identify the floor system. State epoxy/urethane coating, cement-resin, bare concrete, tile or other finish; include coating condition, joints, repaired areas and wet/oily zones. Obtain the floor supplier's own cleaning and damage limits.
  3. Qualify the exact tread. Request compound identity, hardness and test method, tread profile, core/bond construction, and manufacturer evidence for the specific chip type. A generic “PU”, “rubber”, “non-marking” or “floor-protective” label is insufficient.
  4. Remove overload as a confounder. Confirm actual maximum wheel reaction, including uneven floor, load shift, AGV acceleration and turning. The Bodyweld case itself involved equipment over the stated caster rating; do not use a softer tread to mask an undersized caster.
  5. Validate on the real route. If the supplier's evidence does not match the site, agree a controlled sample trial using the actual chip, floor, load, speed, turning pattern and shift duration. Inspect tread pickup/embedding, floor scoring, rolling resistance, tracking and tread damage at agreed intervals. This is a proposed buyer acceptance method, not a test already performed by this supplier.
  6. Set a cleaning and inspection control. Define who removes chips, how often the route is swept, and how wheels are inspected/cleaned. ErgonArmor's at-least-daily dry-sweep recommendation is a coating-specific reference, not a substitute for the actual site's risk-based schedule.

RFQ and substitution questions

  • Which exact tread compound, hardness (including Shore scale and test method) and tread profile are supplied?
  • What metal-chip / weld-slag type, particle dimensions and contamination level has this exact wheel construction been evaluated against?
  • Does the evidence show debris being deflected, or merely that the wheel material resists abrasion?
  • What are the maximum wheel load, AGV speed, turning frequency, route length and duty cycle used for the evidence?
  • Can the supplier provide before/after tread and floor photographs, test duration, inspection intervals and the acceptance criteria for chip pickup, scoring and tracking?
  • What floor coating system is present, and what cleaning/repair procedure does its manufacturer require?
  • Is the proposed wheel self-produced, stocked or sourced for supply? For third-party models, identify the original manufacturer and exact model; do not represent a sourced model as own production.

Applicability and limits

This comparison supports screening and procurement clarification; it is not a universal material ranking, a certified chip-rejection test, or a prediction of floor life. ELESA+GANTER's recommendation, Caster Connection's field case and Caster Technology's TMP product claim concern different wheel constructions and undisclosed or non-matched operating conditions. Sika and ErgonArmor describe maintenance for their own floor systems. No cross-brand matched test was found, and no metal-chip embedding, floor-groove, AGV tracking or floor-protection test was performed on this supplier's products. No debris-rejection or floor-protection guarantee is claimed.

Sources

  1. ELESA+GANTER, Castors and Wheels — Technical Data, Copyright 2018, printed p.17 §5.1 and floor/covering table, “With chips/obstacles” → rubber; machining residues and floor conditions. Original PDF.
  2. Caster Connection, “Bodyweld: The Right Wheel for the Application”, “Challenge”, “Solution” and “Results”; accessed 2026-11-25. Original case study.
  3. Caster Technology Corporation, “Wheels”, TMP Series, “Soft Rubber on Polyolefin, Crowned Tread”; accessed 2026-11-25. Original product series page.
  4. Sika, General Maintenance for New Floor Systems — Sikafloor Maintenance Guidelines, p.1, “Sikafloor Maintenance Guidelines”; document revision date not visible in the retrieved copy, accessed 2026-11-25. Original PDF.
  5. ErgonArmor, Technical Bulletin T21-010, 2021-08-31, p.1, “Maintenance Suggestions: Epoxy & Urethane Floor Coatings”. Original bulletin PDF.