Buyer decision guide · 2026-11-25

Does a −40°C polyurethane wheel rating prove its tread-to-core bond will survive cold duty?

No. A material temperature range, a room-temperature static adhesion result and a cold-conditioned dynamic wheel qualification are different evidence. Independent joint studies show that temperature, aging/fatigue history and loading direction can change residual strength and even where the joint fails. They do not provide a failure prediction for a caster wheel, but they expose the missing conditions a buyer must ask the wheel supplier to qualify.

The buyer decision

For a polyurethane tread bonded to a wheel core, do not approve a freezer or cold-to-warm application from a “−40°C” material statement or a room-temperature pull-off value alone. Require the supplier to identify the exact tread/core construction and show that the bond remains acceptable after the actual cold soak, loaded cycles and temperature transitions. Ask not only how much force the specimen carried, but also where it failed: within the polyurethane, at the polyurethane/adhesive interface, within the adhesive/primer, or at the primer/core interface.

This is a narrower question than whether a caster can operate at −40°C. The wheel material, tread-to-core bond, bearing grease, swivel grease, seals and condensation management are separate qualification items. This guide addresses the bond interface only; it does not replace the complete-caster checks in the low-temperature wheel-rating guide.

What the sources actually establish

Independent sourceOriginal evidence and locationWhat it does not prove
Tan et al., International Journal of Adhesion and Adhesives (2021), Vol. 107, Article 102819Abstract and “Materials”: Sikaflex®-265 one-component polyurethane adhesive bonded to 6005A aluminium alloy in thick-adherend shear-joint specimens. “Failure load and failure displacement analysis” / “Fatigue temperature analysis” and “Conclusions”: quasi-static temperatures −40, −10, 20, 50 and 80°C; fatigue load levels 60%, 50%, 40%, 30% and 20%; adhesive-layer temperature increased with fatigue frequency. The authors report interface failure as easier at low temperature and cohesive failure as easier at high temperature. At 80°C, failure load and displacement were respectively 76.88% and 57.36% lower than at −40°C for this particular joint system.This is a structural adhesive joint using a named adhesive and aluminium substrate, not a cast polyurethane wheel tread bonded to a metal or polymer hub. Its percentages and failure behaviour cannot be assigned to a caster wheel.
Chen et al., International Journal of Adhesion and Adhesives (2023), Vol. 123, Article 103344Abstract and “Residual strength analysis”: polyurethane elastomeric bonded joints were examined after 0, 20, …, 120 hygrothermal aging cycles, at service temperatures from −40 to 80°C and loading angles from 0° to 90° in 15° steps. The reported lowest residual-strength condition combined 120 aging cycles, 80°C and 90° loading. The authors report that aging patterns were not consistent across the different test conditions.The paper studies bonded joints, not a caster wheel. The combined worst case does not mean 80°C/90° is the universal worst condition for every wheel bond, nor does it quantify a −40°C wheel rating.
HAMMER CASTER, Products Catalogue No.52-1“Cold resistant casters”, printed p.26: cold-resistant temperature is referenced from wheel-material characteristics; the catalogue warns that physical properties generally degrade at low temperature and breakage/damage becomes more likely. It separately lists swivel grease, wheel grease and (if fitted) dust-proof seal as items to change, and warns that condensation can freeze after movement from a cold to a warmer environment.This is manufacturer cold-storage guidance, not a tread/core bond test or an adhesive-strength specification.
MHI / Institute of Caster and Wheel Manufacturers, Casters, Wheels and Accessories Guide 101Printed p.14, “Main wheel types”: polyurethane wheel treads are described as chemically bonded to a caster iron core; polyurethane wheel types include open-cast and injection-moulded constructions.This is an industry description of a construction family, not a universal statement that every PU wheel uses the same bond chemistry, core preparation or acceptance test.

Cross-source analysis: temperature is not a one-dimensional bond rating

The 2021 study shows why a single room-temperature bond number is incomplete. Under its specific Sikaflex®-265/aluminium joint setup, the failure mode shifted with temperature: interface failure was more likely at low temperature, while cohesive failure was more likely at high temperature. Its quasi-static failure load also changed substantially across the temperature range, and its fatigue work separately examined load level and frequency. This means a buyer should distinguish bond strength from failure location and fatigue durability.

The 2023 study adds a second dimension. It varied aging cycles, service temperature and loading angle rather than treating temperature as the only variable. Its lowest residual strength occurred at the combined 120-cycle / 80°C / 90° condition, and the authors report inconsistent aging patterns across conditions. Therefore, the lowest ambient temperature is not automatically the only or worst bond condition; a temperature-only coupon result can miss the effect of aging and load direction.

The caster-specific sources establish why this matters in a wheel. HAMMER CASTER says low-temperature material characteristics do not prevent general physical-property degradation and warns about breakage; the ICWM guide confirms that chemically bonded polyurethane-to-iron-core construction is used in the caster industry. Separately, Caster Concepts' existing wheel-specific model describes heat generated by cyclic tread deformation under load and speed, and limits its model to thin PU treads and bounded deflection. The wheel's bond therefore sits inside a real combination of tread deformation, hub interface, temperature and duty—not an isolated room-temperature pull specimen.

New conclusion: cold-storage tread-bond approval needs at least two distinct evidence layers: (1) a static bond/process screen that identifies the specimen, test direction, rate, acceptance threshold and failure location; and (2) a cold-conditioned, cyclically loaded wheel or representative assembly qualification that reproduces the application's temperature sequence, load direction, speed/duty and aging or transition history. A “strong bond” result without the second layer does not establish cold-duty retention.

What can and cannot be compared

  • The 2021 and 2023 studies are independent polyurethane-joint investigations, but their substrates, adhesives, specimen geometries, loading schedules and ageing protocols are not a shared head-to-head test. Do not compare their absolute strength values or treat their failure conditions as interchangeable.
  • The 2021 result that interface failure is easier at low temperature is specific to its Sikaflex®-265 / 6005A aluminium joint. It is a warning to inspect interface failure mode, not proof that a caster tread will delaminate at −40°C.
  • The 2023 minimum residual-strength condition combines aging, high temperature and high loading angle. It demonstrates a multi-variable test envelope; it does not establish the coldest condition as the weakest or a universal load-angle rule.
  • HAMMER's catalogue values are based on wheel-material characteristics and do not report bond testing. The catalogue's grease, seal and condensation changes remain separate complete-caster issues.
  • No source found in this round reports a matched set of caster wheels tested with the same tread compound, hub material, bond process, cold-soak duration, load, speed, temperature transitions and acceptance criteria.

RFQ and substitution-approval requirements

  1. Identify the construction: exact wheel manufacturer/model, tread compound and process (cast elastomer or TPU), tread thickness/profile, core material, surface preparation, primer/adhesive system and any mechanical key or undercut. “PU bonded to core” is not a complete construction description.
  2. Document process state: request the bond-system identity, surface-cleaning/preparation method, primer/adhesive application, cure and post-cure conditions, and conditioning time before testing. Do not ask for proprietary trade secrets where the supplier cannot disclose them; require a controlled process declaration and product-specific evidence instead.
  3. Define the cold duty: minimum temperature, cold-soak duration, loaded time at temperature, cold/warm transition count, drying/condensation conditions, recovery interval and whether the wheel is struck or turned while cold-soaked.
  4. Define the mechanical duty: per-wheel load, speed, duty cycle, driven or free-wheeling operation, acceleration/braking, turning and side-load direction, obstacle/impact sequence, floor and contamination conditions.
  5. Request static bond evidence: method, specimen geometry, substrate and adhesive system, test temperature, loading direction/rate, sample count, numerical acceptance threshold and failure-location classification. A result without failure mode is incomplete for an interface-sensitive application.
  6. Request cold dynamic evidence: test the exact finished wheel or a representative assembly after the specified cold soak and repeated load cycles. Record wheel size, load, speed, cycle schedule, temperature at the bond region if measured, post-test edge lift/cracking/separation and retained rolling function. If only coupon data exist, record the finished-wheel bond qualification as unverified.
  7. Keep complete-caster checks separate: confirm wheel-bearing grease, swivel grease, seals and condensation handling independently; a successful tread bond does not prove cold start or swivel rotation.

Practical substitution rule: if the proposed wheel's “−40°C” claim is only material guidance, or its bond result is a room-temperature static coupon without failure-mode and cold-cycle evidence, classify the substitution as not yet qualified for cold dynamic duty. This is a hold for missing evidence, not a declaration that the wheel will fail.

Scope and evidence limits

The academic studies concern polyurethane adhesive joints and provide mechanism/qualification context only. Their numerical strengths, percentages, temperatures and cycle counts must not be transferred to molded caster-wheel tread bonds. The cited caster sources do not publish a common cold-conditioned tread/core bond protocol or pass/fail threshold. No supplier-specific wheel construction, adhesive system, bond-strength result, low-temperature cycling test or −40°C tread-retention guarantee is established here. No test was performed on products supplied by this business.

Sources

  1. Wei Tan, Jingxin Na, Guangbin Wang, Qianhui Xu, Hao Shen and Wenlong Mu, “The effects of service temperature on the fatigue behavior of a polyurethane adhesive joint”, International Journal of Adhesion and Adhesives, Vol. 107, June 2021, Article 102819, DOI 10.1016/j.ijadhadh.2021.102819; Abstract and sections “Materials”, “Failure load and failure displacement analysis”, “Fatigue temperature analysis” and “Conclusions”. Original article
  2. Hongli Chen, Dengfeng Wang, Jingxin Na, Xin Chen and Huan Meng, “Strength evaluation of polyurethane elastomeric bonded joints under extreme service conditions”, International Journal of Adhesion and Adhesives, Vol. 123, April 2023, Article 103344, DOI 10.1016/j.ijadhadh.2023.103344; Abstract and “Residual strength analysis”. Original article
  3. HAMMER CASTER, Products Catalogue No.52-1, “Cold resistant casters”, printed p.26. Original catalogue
  4. MHI / Institute of Caster and Wheel Manufacturers, Casters, Wheels and Accessories Guide 101, printed p.14, “Main wheel types”. Original guide
  5. Caster Concepts, Doug Backinger, “Predictive Product Failure Model for Polyurethane Treaded Wheels Based on Load and Speeds”, published 2025-02-21, “Heat generation”, “Results” and “Conclusions”; used only for caster-wheel context, not counted as an independent adhesive-joint experiment. Original manufacturer article